Home / Hardscape Materials and Product Choices / Polymeric sand explained

Polymeric sand vs regular joint sand

Polymeric sand is a stabilized joint sand, a product choice rather than a requirement. The industry’s own maintenance guide treats it carefully: it can be used during construction, it is not recommended for topping up joints, and it does not belong in permeable pavers.

What the industry standard calls for

The base specification for interlocking concrete pavers from the Concrete Masonry and Hardscapes Association (CMHA, which includes ICPI) calls for dry sand meeting ASTM C144 or CSA A179 in the joints, often called mason sand. Bedding sand may also be used as joint sand. Joint widths are 1/16 to 3/16 in. (2 to 5 mm), and CMHA’s maintenance guide gives an optimal joint width of 1.5 to 3 mm (0.05 to 0.12 in.). A plain-sand joint is the baseline against which polymeric sand is compared. Our own steps for filling joints are on how to compact pavers and fill joints, and the glossary has joint sand defined.

What CMHA says about polymeric and stabilized sand

CMHA’s Operation and Maintenance Guide uses the term stabilized sand and makes four points:

  • Stabilized sand can be used during construction to reduce joint sand loss.
  • Polymeric sand is not recommended for topping up joints later.
  • Sealers can also help hold sand in joints; they are applied as a liquid over the paver surface and must soak in and cure.
  • Stabilized sand is harder to remove when pavers are lifted and reinstated, so recycling the pavers may cost more.

That last point is the trade-off a homeowner should hear. If you expect to open the patio later for a utility repair, stabilized joints make the work harder.

Why joints lose sand in the first place

CMHA says joint sand loss commonly results from pressure washing, or from saturated bedding sand that pumps up through the joints under traffic. Both involve water, which is why drainage, base and slope matter. If the joints keep emptying, look at the base and bedding before reaching for a different joint product. See paver patio slope for drainage.

Plain sand or polymeric sand: how to decide

QuestionPlain mason sandPolymeric / stabilized sand
Source of the specASTM C144 in the guide specificationProduct choice; CMHA allows stabilized sand during construction
Top-up laterYes. Add dry sand when joints drop more than 1/2 in. below the surfaceCMHA does not recommend it for topping up
Removal during repairsNot flagged as a problem by CMHAHarder to remove, per CMHA
Permeable paversNo: CMHA specifies angular No. 8, 89 or 9 stoneNo: CMHA specifies stone, not sand, in the openings

Maintenance that applies either way

  • Inspect twice a year: in spring during or just after rain, and in late summer or early fall.
  • Top up when joint sand drops more than 1/2 in. (12 mm) below the paver surface.
  • Spread dry masonry sand to the bottom of the chamfers, remove the excess, then compact with at least two passes of a plate compactor rated 5,000 lbf or more and re-spread until the joints stop taking sand.

Questions to ask your installer

  • Are you using plain sand or a stabilized sand in the joints, and why?
  • What does the product label require for dryness, weather and sealer timing? Follow it exactly; we did not find a neutral industry standard for those details.
  • If we need to lift pavers later, what will that cost compared with plain sand?
  • What joint width are you building to?

For quantities, use the joint sand and sealer calculator. For timing around sealing, see how long to wait to seal pavers.

Related

All hardscape materials · Permeable interlocking pavers · Concrete pavers explained

Get a quote

FAQ

Is polymeric sand required for pavers?

No. The CMHA guide specification calls for dry sand to ASTM C144 in the joints. Stabilized sand is an option CMHA says can reduce joint sand loss during construction.

Can I top up old joints with polymeric sand?

CMHA’s maintenance guide says polymeric sand is not recommended for topping up joints. It advises adding dry masonry sand when the joints drop more than 1/2 in. below the surface.

Why does joint sand wash out?

CMHA says it commonly results from pressure washing or from saturated bedding sand that pumps up through the joints under traffic.

Can I use polymeric sand in permeable pavers?

No. CMHA specifies angular stone in the joint openings and an open-graded stone bedding course for permeable pavements, not sand.

Planning information only, not engineering advice. Product directions vary by manufacturer; follow the label and your installer’s instructions. Sources checked Nov 23, 2026.