What Is Spalling? Concrete and Paver Surface Flaking Defined
Spalling (or a spall) is the flaking, chipping or peeling away of the surface of concrete, pavers or masonry. It leaves a rough, pitted patch where the surface layer used to be.
What spalling means
Spalling happens when the surface is pushed off by pressure from within. In cold climates the usual cause is water soaking in, freezing and expanding, a cycle that repeats all winter. De-icing salts can make the damage worse on concrete surfaces. Manufacturers and industry groups publish guidance on which de-icers to avoid.
Where it comes up
It comes up on steps, driveways, walkways and pavers after winter, and in warranty claims. Spalling is a surface condition, which is different from the white haze of efflorescence, a deposit that can be cleaned off.
In the field
Units that meet ASTM C936 have freeze-thaw requirements, and good drainage keeps water from sitting. See also should you seal pavers. Badly spalled units generally need to be replaced. Surface repair is not a long-term fix.
Spall versus scaling
CMHA defines a spall as a flake-shaped fragment that breaks off a unit’s edge or surface, and lists causes such as a sharp blow, weathering or pressure from neighboring units. On poured concrete flatwork the related surface failure is usually called scaling. The Pennsylvania Concrete Association describes it as surface damage that often shows up in spring on driveways and sidewalks, common in Northeast climates.
Why concrete flakes
An FHWA pavement brief explains that freeze-thaw damage is worst when concrete is saturated. Concrete above roughly 85 percent saturation can be damaged within a few cycles, while partly dry concrete generally is not. De-icers raise saturation and add other stresses, which is why salt makes winter damage worse. The same brief ties joint spalling to an inadequate entrained air-void system, with air content targets of 4 to 6 percent for moderate exposure and 4.5 to 7.5 percent for severe exposure, and a maximum water-to-cementitious ratio of 0.45.
Common mistakes on flatwork
- Overworking the surface. The Pennsylvania Concrete Association says not to start finishing while bleed water is still visible, and never to add water to the surface.
- Skipping protection in cold weather. Concrete placed in late fall or winter should be kept above freezing until it reaches design strength, typically around 28 days.
- Salting new concrete. The association generally recommends no de-icers in the first year, and the FHWA brief suggests at least a 30-day drying period after curing before any de-icer is used. It specifically calls ammonium sulfate and ammonium nitrate too aggressive for concrete.
- Skipping curing. Curing compounds and sealers hold moisture in so the slab keeps gaining strength, and sealers also slow chloride-laden water from getting in.
Related terms: bleed water, air-entrained concrete, paver and control joint. Added details come from the Pennsylvania Concrete Association scaling sheet, an FHWA concrete pavement brief and CMHA PAV-TEC-001.
Frequently asked questions
What causes spalling?
Most often freeze-thaw cycles in water-saturated surfaces, sometimes made worse by de-icing salts.
Is spalling the same as efflorescence?
No. Efflorescence is a white mineral deposit on the surface. Spalling is the surface itself breaking away.
Can spalled pavers be repaired?
Individual damaged pavers can usually be lifted and replaced with matching units.
Sources
- CMHA, PAV-TEC-001: Glossary of Terms for Segmental Concrete Pavement (2023)
- ASTM C936: Standard Specification for Solid Concrete Interlocking Paving Units
Related
- Hardscape glossary
- Related terms: frost heave and ASTM C936
- Should you seal pavers
Dealing with damaged pavers in central PA? Contact Muthler Landscaping & Construction for a straight answer.