Skip to content Groundwork Design Co.Want a design?Custom patio, wall, deck and yard plans, drawn by builders. Anywhere in the U.S. From $349.Start here
LOCK HAVEN, PA · PA HIC #PA212584 · INSURED FREE ESTIMATES · CALL OR TEXT
PAGE

What Is Air-Entrained Concrete?

Air-entrained concrete is concrete made with an admixture that creates billions of microscopic air bubbles, which give freezing water room to expand without cracking the surface.

What the bubbles do

An FHWA pavement guide describes entrained bubbles as very small, about 0.01 to 1 millimeter across. They improve freeze-thaw durability and resistance to deicer scaling, which is why exterior concrete in cold regions such as central Pennsylvania is normally air-entrained. Without it, water in the surface freezes and flakes the top layer off.

The trade-offs

FHWA says each 1 percent of air reduces 28-day compressive strength by about 3 to 5 percent, so air content is controlled within a range rather than maximized. NRMCA adds that air-entrained concrete bleeds less and generally should not be steel-troweled, because that can seal the surface and lead to blisters. A wood or magnesium float and a broom finish are typical on exterior slabs.

Planning information only. Required air content comes from your mix design and the supplier.

Entrained air versus entrapped air

FHWA’s resource separates two kinds of voids. Entrained bubbles are spherical and added on purpose during mixing, usually with a surface-active agent. Entrapped voids are irregular, typically larger than 1 mm, present in all concrete and less useful. FHWA also explains that air-entraining admixtures do not create bubbles by themselves. They lower the surface tension of the mixing water and form a shell that stabilizes bubbles and hinders them from merging. Smaller, better-distributed bubbles shorten the distance water has to travel to reach a void and relieve pressure.

Why freezing damages concrete without it

FHWA says concrete becomes critically saturated above about 91.7 percent saturation, and that ice expands about 9 percent by volume. If the pressure exceeds the tensile strength of the paste, the concrete cracks. Entrained voids give the freezing water room to move, which relieves that pressure. Air entrainment is also credited with improving resistance to scaling from deicing salts, the surface flaking that the blisters page separates from blistering.

What changes the air content before the slab is finished

Air does not stay constant from the batch plant to the form. FHWA lists cement, supplementary cementitious materials, aggregates, chemical admixtures, the water-cementitious ratio, batching and mixing, transport, placing, finishing and concrete temperature as influences. It lists belt conveyors, pumping (with the strongest effect), prolonged internal vibration and excessive finishing as practices that decrease air content. It also notes that water reducers and high-range water reducers increase air content, and that admixture dosage must be adjusted for these factors. For a small driveway or patio, the takeaway is to tell the supplier how the concrete will be placed so the mix is ordered with that in mind.

Common mistakes

NRMCA’s blister bulletin warns against steel troweling air-entrained normal-weight concrete and against applying dry-shake hardeners to it too early, because air-entrained concrete bleeds less and can look ready sooner than it is. Overworking the surface can also lower the air at the top, per FHWA’s list of finishing effects. The bulletin recommends non-air-entrained concrete for interior slabs, so the mix used for a garage floor or basement slab may differ from the one used for an exterior patio. Planning information only; confirm the air requirement for your slab with your supplier and your local code office.

Related terms: frost heave and spall. Sources for this section: FHWA, HIF-20-085 and NRMCA CIP 13.

FAQ

Do patios and driveways need it?

In areas with freezing winters and deicers, exterior flatwork is generally air-entrained. Ask your supplier to confirm the mix.

Does it make concrete weaker?

Slightly. FHWA puts it at about 3 to 5 percent less compressive strength per 1 percent air.

Can I add air later?

No. It is added to the mix at the batch plant or truck, not to hardened concrete.

Sources

Related

Back to the full glossary. Related terms: Bleed water and Slump.