What Are Blisters in Concrete?
Blisters are hollow bumps on a concrete surface, roughly ¼ inch to 4 inches across, covered by a thin skin of mortar.
What they are
NRMCA describes blisters as hollow bumps about ¼ to 4 inches wide with a skin around ⅛ inch thick. The skin is the top of the slab, sealed by finishing, with trapped air or bleed water underneath. They often break off under traffic and leave a pitted spot.
Causes and prevention
NRMCA points to troweling too early as a common cause, which seals the surface while water and air are still rising. Its prevention advice includes keeping slump in a moderate range, since a vibratory screed on a mix over 5 inches of slump can push aggregate down. It also says air-entrained concrete generally should not be steel-troweled. Waiting until bleeding has stopped before the final finishing pass is the simple rule.
Planning information only. Repairs and finishing timing depend on the slab, so ask your concrete contractor.
Why the top seals before the slab is ready
NRMCA explains that the top surface can stiffen or set faster than the concrete beneath it. Trapped air or bleed water then migrates upward and collects under the sealed surface. Several site conditions push in that direction. Fast evaporation from heat, low humidity or wind can make the top look ready while bleeding continues. A subgrade cooler than the concrete and air makes the top set faster than the base. Higher entrained air reduces bleeding, which falsely signals readiness, and thicker slabs take longer for air and water to rise. Small blisters can be hard to see in poor lighting and may not show until they break under traffic.
Finishing habits that raise the risk
The bulletin lists several. Too little vibration leaves air in the mix, and too much, especially with vibrating screeds on high-slump concrete, pushes aggregate down and brings mortar up. Float pans can start finishing too early because of their weight. Tilting trowel blades on second or third passes pushes air and water under the surface, which is why NRMCA recommends flat float and trowel blades. Dry-shake hardeners applied too early, particularly on air-entrained concrete, contribute as well. So does placing a slab directly on a vapor retarder or a saturated base, since the bleed water cannot drain into the subgrade. NRMCA notes that its guidance on wood versus metal floats for air-entrained concrete is unclear, so confirm tool choice with your finisher.
Prevention in cold and hot conditions
Under high evaporation, NRMCA suggests covering the slab with plastic sheeting or using fog sprays or evaporation retardants. If the surface crusts, adjust finishing to keep it open and avoid folding air in. In cold weather, it says to heat the subgrade, keep the concrete above 50°F and consider an accelerating admixture. It also says to plan crew size so finishing is not started too early on any section.
Repair limits
NRMCA says blisters are hard to repair once the concrete hardens. Options it names include eliminating and rebonding the blistered areas or opening the surface with a wood tool, and it says climate or mix issues may need correcting so the problem does not return. Larger affected areas are called delamination in its terms. For more on finishing, NRMCA points to ACI 302.1R. Planning information only; your concrete contractor decides the repair for your slab.
Related terms: spall and control joint. Source for this section: NRMCA CIP 13.
FAQ
Are blisters the same as scaling?
No. Blisters are raised bumps that form during finishing. Scaling is flaking off of the surface later, often from freezing and deicers.
Can they be repaired?
Yes, usually by removing the loose skin and patching. Prevention is cheaper.
Why not trowel early to finish faster?
It is the most common way to create them.
Sources
Related
Back to the full glossary. Related terms: Bleed water and Slump.
Planning a concrete slab or driveway? Contact Muthler Landscaping & Construction.