DSA driving surface aggregate
Quick answer: Penn State describes DSA as 2A-like road surface stone with 10 to 17 percent fines, PI 0 to 4, maximum abrasion 40 and maximum soundness 20 percent. The 2020 bulletin and 3/2025 handbook show slightly different gradation rows.
What DSA is
DSA stands for driving surface aggregate. The Penn State Center for Dirt and Gravel Roads Studies describes it in its Aggregate 101 bulletin (copyright 2020) as similar to PennDOT 2A, but with more fines and extra requirements for resistance to the wear and erosion that road surfaces take. Both Penn State documents list it as an unbound road surface material. Appendix F ties it to the Dirt and Gravel Road Maintenance Program, and nothing I read presents it as a Pub 408 class or gives it a Pub 408 section number.
The numbers Penn State gives
Aggregate 101 gives these DSA figures: fines of 10 to 17 percent, a maximum Los Angeles abrasion value of 40, a maximum soundness loss of 20 percent and a plasticity index range of 0 to 4. A footnote says DSA may carry up to 17 percent fines if the PI is below 2. The row in the gradation table lists a 1.5 inch top size and reads 100, 65 to 97, 30 to 65, 15 to 30, then 10 to 15, with an asterisk on the last value.
Appendix F of the 3/2025 DSA Handbook shows a different row: 100, 65 to 95, 30 to 65, 15 to 32, then 11 to 15. Three of the five ranges differ between the documents: 65 to 97 versus 65 to 95, 15 to 30 versus 15 to 32, and 10 to 15 versus 11 to 15. The 2020 bulletin is the older of the two, so the newer handbook may reflect an update, but neither says so. I am not choosing between them. Also, in both documents the sieve headers do not line up cleanly with the five values, so I cannot tell you which sieve each range applies to. Use the DSA Handbook itself or the current program specification for sieve limits.
DSA compared with 2A
Appendix F lists 2A as 2 inch material for road base and road surface with a longer row of values: 100, 52 to 100, 36 to 70, 24 to 50, 16 to 38, 10 to 30, then 0 to 10. Aggregate 101 says PennDOT 2A allows 0 to 10 percent fines and DSA allows 10 to 17 percent. So the two stones overlap in use, but DSA has a smaller top size at 1.5 inch and a higher fines range. See PennDOT 2A subbase stone for the 2A side.
Appendix F adds that 2A is the most common aggregate people modify, meaning they blend fines into it, and that PennDOT no longer has a modified specification. If a road crew says they use modified 2A, that is a local practice, not a current PennDOT class.
Why the fines go up
Aggregate 101 explains the basics. Fines are particles smaller than the No. 200 sieve, about 0.003 inch or 0.075 mm, found by washing the sample, and fine content decides whether an aggregate is open or well graded. Well-graded material has few air voids, compacts better and is preferred for road surfaces. Open-graded material drains but does not compact into a dense mass. A road surface that has to hold together under traffic is therefore a better fit for the well-graded side. The bulletin implies this is the reason for DSA’s higher fines, though it does not state it in those words.
Why plasticity stays low
The plasticity index estimates the clay content of the fine material. Aggregate 101 says a PI above about 6 makes the material behave more like a cohesive soil than an aggregate, and that high clay can hold moisture and cause deformation and rutting in surface layers. Appendix F says surface aggregates should ideally be non-plastic to slightly plastic with a PI of 6 or lower. DSA’s 0 to 4 range sits inside that guidance, and the footnote lets fines climb to 17 percent only when PI is below 2. As I read the two documents, that is how a stone with this much fine material is kept workable as a surface: the fines have to be low in clay.
Durability tests
Aggregate 101 says LA abrasion measures wear resistance, where lower is better, and matters most for road surfacing. Soundness uses a sodium sulfate test that mimics ice crystal growth, matters most for material on the surface or buried less than 24 inches deep, and also reads lower is better. Both depend on the parent rock rather than how it is crushed. The bulletin calls limestone the hardest common source and shale the softest. DSA’s limits are 40 for abrasion and 20 percent for soundness. Appendix F lists PennDOT Types A, B and C at 10, 12 and 20 percent soundness and 40, 45 and 55 abrasion. The Course Book copy of Pub 408 Table B shows Type A abrasion at 45, so the Penn State sources disagree about Type A, and the edition in your documents controls. See aggregate quality types A, B, C and S.
Testing and certification
Aggregate 101 says DSA is tested by Conservation Districts or the Center before purchase. Appendix F says that on Dirt and Gravel Road Maintenance Program projects, a certification must accompany the first load each day. If you are bidding or building on a program road, confirm the testing and certification steps with the conservation district.
What the sources do not say
In the parts I read, neither document gives a DSA lift thickness, a compaction target, a crown or a cost. Appendix F does not name LA abrasion or give DSA-specific soundness limits in its own text, and the bulletin’s narrative does not explain how DSA and 2A compare on traffic. Those details may be in the program specification, which I did not read. Also note Aggregate 101 says 2RC is cheap and fine for pipe bedding or fill but is a weaker choice for surfacing because of its clay content. See PennDOT 2RC.
Editions
Aggregate 101 carries a 2020 copyright, and the text suggests a January 2021 printing. Appendix F is dated 3/2025. The Pub 408 values quoted for comparison come from the 2020 edition, Change No. 2, as copied in the Penn State Aggregate Course Book 2022-23. I did not read the 2026 edition.
Common mistakes
- Specifying DSA as if it were a Pub 408 class.
- Quoting one gradation row without noting the two Penn State documents differ.
- Allowing 17 percent fines without checking PI.
- Assuming modified 2A is a current PennDOT specification.
Sources
- Penn State Center for Dirt and Gravel Roads Studies, Aggregate 101 technical bulletin (copyright 2020)
- Penn State, DSA Handbook Appendix F (3/2025)
- Penn State Aggregate Course Book 2022-23 (copies Pub 408/2020 Change No. 2, Sections 703 and 704)
Related
All aggregates · PennDOT 2A subbase · PennDOT 2RC · Open vs dense graded
FAQ
What is DSA aggregate?
Driving surface aggregate is Penn State’s unbound road surface stone, similar to PennDOT 2A with more fines (10 to 17 percent) and added wear and erosion requirements.
How is DSA different from 2A?
DSA has a 1.5 inch top size and 10 to 17 percent fines. Penn State lists 2A as 2 inch material with 0 to 10 percent fines.
What PI does DSA allow?
Aggregate 101 gives a plasticity index range of 0 to 4, with up to 17 percent fines only if PI is below 2.
Do the Penn State sources agree on the DSA gradation?
Not exactly. The 2020 bulletin and the 3/2025 handbook show slightly different ranges, so confirm against the current specification.
Planning information only. The project specification and your engineer or inspector govern. Sources checked Nov 23, 2026.