Skip to content Groundwork Design Co.Want a design?Custom patio, wall, deck and yard plans, drawn by builders. Anywhere in the U.S. From $349.Start here
LOCK HAVEN, PA · PA HIC #PA212584 · INSURED FREE ESTIMATES · CALL OR TEXT
PAGE

What Is Efflorescence? The White Powder on Block, Brick and Concrete

Efflorescence is the white, powdery or crusty deposit that shows up on the surface of brick, concrete block, pavers, stone and concrete. It is left behind when water carries soluble salts out of the material and then evaporates. It is mostly a cosmetic problem, but it tells you water is moving through the wall or slab, and that is worth tracing.

Efflorescence and the terms around it

  • Efflorescence: per the Concrete Masonry and Hardscapes Association (CMHA), a usually white deposit of soluble salts and bases on a masonry or concrete surface. CMHA says it is mainly an aesthetic concern and does not affect structural performance.
  • New building bloom: the Brick Industry Association’s name for efflorescence in the first year. It usually comes from salts and moisture left over from construction and tends to fade.
  • Leachate or lime run: CMHA’s name for heavy white streaks below mortar joints. It signals ongoing water entry, not just early-age drying.
  • Subflorescence: salts that crystallize beneath the surface instead of on it. The Brick Industry Association warns that trapped salts can exert enough pressure to spall brick.

Why it matters on a job

Homeowners call about white stains on a new retaining wall, a block planter or a paver patio all the time, and the first question is always whether something is wrong. Usually it is not structural. Both CMHA and the Brick Industry Association describe it as undesirable but generally not harmful. The useful question is why the water is there.

Timing is the clue. Efflorescence in the first year is often leftover construction moisture and salts, and it fades with weather. The Brick Industry Association says efflorescence that appears after a year usually signals water penetration or poor drainage. On a wall, that points us toward the flashing, the caps, the joints and the drainage behind it. On a retaining wall, it points to what the weep holes and drainage zone are doing.

The three conditions

CMHA says efflorescence needs all three of these, and removing any one prevents it:

  • Soluble compounds in the masonry.
  • Moisture to carry the salts to the surface.
  • A driving force, such as evaporation or hydrostatic pressure, to move the solution.

The Brick Industry Association frames it the same way: salts present, water to dissolve them, and pores that let the solution migrate to a surface where the water evaporates. Since eliminating salts completely is impractical, its note focuses mostly on limiting water.

Where the salts and water come from

According to the Brick Industry Association, common salt sources include mortar and grout (where cement alkalis are the main contributor), concrete and concrete masonry backing, stone and precast trim, soil and groundwater, and sometimes the brick itself. It notes that concrete products can contain two to seven times as much soluble material as fired clay. CMHA adds that sodium, potassium and calcium compounds in units, mortar, grout and copings and sills can all contribute, and that calcium hydroxide can react with carbon dioxide to leave a whitish calcium carbonate deposit.

For water, CMHA lists rain entering through permeable units, partially filled joints, flashing failures and cracks, interior vapor condensing in the wall, water entering during construction, and groundwater rising by capillary action. It also says efflorescence is more common in winter, when slow evaporation brings salts to the surface, and that spring warming can release frozen moisture and mobilize more salts. That matches what we see after a Pennsylvania winter.

How to prevent it

The two sources agree on the priorities. Verify against the current publications before you write them into a specification.

  • Design to shed water: direct water away from wall tops, use flashing with weep holes where water collects, and use wide overhangs where practical (CMHA). The Brick Industry Association adds sloped trim, fewer joints, and base flashing within 10 inches of grade.
  • Choose clean materials: CMHA suggests considering soluble salt content in units, mortar and grout, and specifying hydrated lime to ASTM C 207, sand to ASTM C 144 and clean mixing water. The Brick Industry Association mentions low-alkali cement with equivalent alkalis limited to 0.60 percent and limiting admixtures of unknown composition.
  • Protect during construction: store materials off the ground and covered, keep mixers and tools clean, protect the top of the wall at the end of each day, and avoid deicing equipment with salt or antifreeze (CMHA). The Brick Industry Association says protective covers should extend 24 inches down each side of the wall and that plastic sheeting thinner than 10 mils is not acceptable as cover.
  • Finish joints well: CMHA recommends concave or vee joints on exposed walls, with head joints fully filled and tooled, and not raked, flush or cut joints. Our mortar joint entry explains the profiles.

How to clean it

Both sources say to fix the moisture source first. Much efflorescence fades with weathering. If it does not, CMHA describes dry brushing and then flushing with clean water, and commercial cleaners following the manufacturer’s directions. The Brick Industry Association says dry brushing usually works, specialty brick cleaners can handle heavier deposits, and any cleaner should be tested on a small area first. It also says to avoid washing except in warm, dry weather, because extra moisture can bring more salt to the surface. CMHA warns against high-pressure water for the same reason.

CMHA treats muriatic acid as a last resort, at a 5 to 10 percent solution, or 2 percent for integrally colored masonry. It says to test a small spot first, wet the wall beforehand, treat no more than 4 square feet at a time, leave the acid about 5 minutes before scrubbing with a stiff bristle brush that is not wire, flush thoroughly afterward, and treat the whole wall to avoid mottling. Acid can damage masonry and hurt skin and eyes, so this is a job for someone with the right protective gear and experience.

Calcium carbonate deposits, CMHA says, are very difficult to remove. Coatings are a different decision. The Brick Industry Association says coatings are not recommended as the sole treatment, because trapped salts can form subflorescence that spalls the surface. CMHA adds that clear water repellents can cause spalling or deposits if the underlying causes are not addressed.

Efflorescence FAQ

Is efflorescence harmful?

CMHA says it is mainly an aesthetic concern and does not affect structural performance. The Brick Industry Association says it is usually not harmful to brick masonry. Heavy or recurring deposits still point to water entry that deserves attention.

Will it go away on its own?

Often, in the first year. Both sources say early efflorescence tends to fade with weathering. If it appears or returns after a year, the Brick Industry Association says it usually signals water penetration or poor drainage.

Should I pressure wash it?

CMHA advises against high-pressure water on walls because it can drive more moisture in. Dry brushing and clean-water flushing are the first steps both sources describe.

Does sealing stop efflorescence?

Not by itself. The Brick Industry Association does not recommend coatings as the sole treatment, since trapped salts can cause spalling. Stopping the water is the real fix.

Sources

Keep reading

White staining on a wall or patio you want checked? Contact Muthler Landscaping & Construction and we will look at where the water is coming from. Planning information, not engineering advice.