Blisters and delamination in concrete slabs

Blisters are hollow bumps on a new slab; delamination is the same problem on a larger scale, where a thin surface layer separates from the concrete below. Both come from finishing the top before the concrete underneath has finished bleeding. The National Ready Mixed Concrete Association (NRMCA) explains the causes and the fixes.

What they are

BlistersDelamination
SizeLow bumps about 1/4 to 4 inches across.A few square inches to many square feet.
StructureA dense mortar skin roughly 1/8 inch thick over a void.A surface layer 1/8 to 1/4 inch thick that breaks off.
How you find themMay break under traffic; small ones are hard to see in poor light.Hollow sound when tapped with a hammer or dragged with a heavy chain; cracking and color differences.

Why they form

Air and bleed water rise through fresh concrete. If the surface is finished too early or stiffens faster than the concrete below, that air and water get trapped under a nearly airtight skin. NRMCA says delamination usually forms late in finishing, after floating and the first troweling pass. Conditions that stiffen the top quickly raise the risk: wind, sun, low humidity, a cold subgrade and rising air temperature.

Conditions that make it more likely

  • A subgrade cooler than the concrete and air, which makes the top set faster than the layers beneath. NRMCA says not to place concrete on a substrate below 40°F.
  • Placing directly on a vapor retarder or a saturated base, which blocks bleed water from draining down.
  • Higher-than-normal air content, which reduces bleeding so the surface seems ready sooner than it is. NRMCA says air-entrained concrete should not be specified for hard-troweled slabs, and recommends a maximum of 3 percent air for troweled floor slabs.
  • Too much or too little vibration, jitterbugs, or vibrating screeds on higher-slump concrete.
  • Dry-shake hardeners applied too early, and sticky mixes with high cement, sand or fines content.

This matters for outdoor work too. Exterior slabs in freeze-thaw country normally are air-entrained (see 3000 vs 4000 psi concrete), which is why NRMCA says not to steel-trowel air-entrained concrete and why a broom finish is the usual exterior texture.

Prevention rules

  • Do not over-consolidate or seal the surface before trapped air and bleed water have escaped.
  • Delay final finishing as long as possible. NRMCA gives a boot indentation of about 1/4 inch as a sign of sufficient stiffening, and says to probe to confirm the concrete below is not still plastic.
  • Use flat blades for initial floating. A surface that tears during troweling is not ready.
  • Do not add excess water at the truck. Keep slump between 3 and 5 inches.
  • In high evaporation, cover with plastic sheeting, use fog sprays or apply evaporation retardants.

Repair

NRMCA says blisters are difficult to repair once the concrete hardens; the blistered areas must be removed and rebonded. For delamination, remove the surface layer, clean the concrete underneath thoroughly, then patch. Extensive delamination may need grinding and a new overlay. Delamination caused by corroding steel near the surface is a separate, thicker problem.

Sources

Related

Finishing concrete flatwork · Dusting and crazing · All concrete guides

Get a quote

FAQ

What causes blisters on a concrete slab?

NRMCA says air or bleed water migrates upward and gets trapped under a surface sealed by premature or excessive troweling.

How can I tell if a slab is delaminated?

NRMCA says a hollow sound when tapped with a hammer or dragged with a heavy chain, along with cracking or color differences, indicates delamination.

Can blisters be repaired?

NRMCA says blisters are difficult to repair once concrete hardens. The affected areas must be removed and rebonded.

Does air-entrained concrete cause delamination?

It raises the risk in troweled slabs because it reduces bleeding. NRMCA says not to specify air-entrained concrete for hard-troweled slabs.

Planning information only, not engineering advice. Have a qualified professional evaluate a specific slab. Sources checked Nov 23, 2026.