Skip to content Groundwork Design Co.Want a design?Custom patio, wall, deck and yard plans, drawn by builders. Anywhere in the U.S. From $349.Start here
LOCK HAVEN, PA · PA HIC #PA212584 · INSURED FREE ESTIMATES · CALL OR TEXT

Home / Compare / Brick vs concrete pavers

Comparison · central PA

Brick vs concrete pavers

Clay brick pavers and concrete pavers are covered by two different ASTM standards, and the numbers do not line up one for one. The concrete standard, ASTM C936, asks for an average compressive strength of at least 8,000 psi and an average absorption of no more than 5 percent. The clay standard, ASTM C902, sets limits by class, and its top class, SX, also uses 8,000 psi but allows up to 8 percent absorption. The Brick Industry Association says clay color is fired through the unit and does not fade, while the Concrete Masonry and Hardscapes Association says concrete color changes gradually at the surface. None of the sources gives a price comparison or a central Pennsylvania field study, so this page compares standards, color and care, not cost.

ASTM C936 (concrete pavers): minimum average compressive strength8,000 psi
Call (570) 397-9800All comparisons

Quick answer

What the sources say, and what they leave out

On paper, SX clay pavers and standard concrete pavers share the same 8,000 psi average strength floor, so strength alone does not separate them. The standards differ on absorption: 5 percent average for concrete under C936, 8 percent average for SX clay under C902. Both have a freeze-thaw path: concrete units exposed to freezing and deicers must show resistance, and clay absorption limits can be waived if five bricks pass ASTM C67. The Brick Industry Association, which represents clay brick makers, says clay resists salt and freezing more consistently than concrete but gives no test data. The concrete association, CMHA, does not discuss clay at all. Where the sources are silent, this page says so. Verify against the current standards and sources.

Side by side

ItemConcrete paversClay brick pavers
StandardASTM C936, solid interlocking concrete paving units (CMHA PAV-TEC-002, revised 2022)ASTM C902, pedestrian and light traffic paving brick (BIA Technical Note 14 excerpt, March 2007, citing the 2006 edition)
Compressive strengthAverage at least 8,000 psi, no unit below 7,200 psi (ASTM C936 sample copy, 2023)Class SX average 8,000 psi, individual 7,000 psi; molded SX 4,000 and 3,500; MX and NX 3,000 and 2,500 (BIA Technical Note 14 excerpt). BIA says most clay pavers exceed 10,000 psi (industry statement)
AbsorptionAverage no more than 5 percent, no unit above 7 percent (ASTM C936 sample copy)SX 8.0 percent average and 11.0 individual; MX 14.0 and 17.0; NX no limit; saturation coefficient limit 0.78 average for SX (BIA Technical Note 14 excerpt)
Freeze-thaw and deicersRequired only if exposed to freezing and deicers; ASTM C1645 mass loss no more than 225 g/m2 after 28 cycles or 500 g/m2 after 49 cycles, tested in 3 percent saline for deicer exposure (ASTM C936 sample copy; CMHA PAV-TEC-002)Absorption and saturation limits can be waived if five bricks pass the ASTM C67 freeze-thaw test with no more than 0.5 percent dry weight loss per unit (BIA Technical Note 14 excerpt). BIA says clay resists salt and freezing more consistently, with no test data given
ThicknessMinimum 60 mm (2 3/8 in.) under C936; ICPI Tech Spec 10 (revised 2015) recommends 60 mm for pedestrian areas and residential driveways and about 80 mm for vehicular pavementsNot covered in the clay sources
ColorPigment is mixed in and cement holds it; traffic, weather and dirt gradually change the surface color (CMHA PAV-TEC-006)Color is fired through the unit and does not fade or need sealers (Brick Industry Association)
EfflorescenceNot structural; can peak as early as 60 days after installation and last for months, and some wears away (CMHA PAV-TEC-005)Possible on brick too: soluble salts may be present in brick, mortar or concrete (Construction Specifier, Howlett, 2012)
SealingSealers help keep water and stains out and may need reapplying; a breathable sealer is advised if efflorescence is a concern (CMHA PAV-TEC-006)BIA says clay does not require sealers for color; it says nothing further about sealing
Edge restraintPlastic or aluminum on flexible or rigid bases, steel on rigid only; timber not recommended; soil backfill never suitable (CMHA PAV-TEC-003)Not covered in the clay sources
RepairIn a utility-cut repair, extracted pavers are stacked aside and reinstated (CMHA PAV-TEC-007)Not covered in the clay sources
PriceNo source compares priceNo source compares price

Concrete Masonry and Hardscapes Association (CMHA), Brick Industry Association (BIA), ASTM C936 sample copy, The Construction Specifier, checked Nov 23, 2026. None of these is a Pennsylvania agency. Verify against current sources and local rules.

What the concrete standard asks for

CMHA’s construction note says U.S.-made pavers should meet ASTM C936, with a minimum average compressive strength of 8,000 psi and an average absorption that should not exceed 5 percent. The sample copy of the 2023 edition adds that no single unit may fall below 7,200 psi or absorb more than 7 percent. Freeze-thaw and deicing-salt durability only has to be shown if the units will actually be exposed to freezing and deicing materials, either through proven field performance or a laboratory test under ASTM C1645. That test allows an average mass loss of no more than 225 g/m2 after 28 cycles or 500 g/m2 after 49 cycles, and units for deicer exposure are tested in a 3 percent saline solution. The same sample sets the minimum thickness at 60 mm, or 2.36 in. ICPI Tech Spec 10 says concrete pavers can resist deicing salts better than conventional paving materials because of their cement content, strength and density, but it gives no test requirement of its own.

What the clay standard asks for

The clay numbers we found come from an excerpt of BIA Technical Note 14 that a paver supplier hosts, and it cites the 2006 edition of ASTM C902, so current limits may differ. It lists Class SX at 8,000 psi average and 7,000 psi individual, with 8 percent average absorption, and molded SX at 4,000 psi with 16 percent. Classes MX and NX drop to 3,000 psi average. It also lists three abrasion types, I through III, by abrasion index and volume loss. The excerpt gives no description of which class is meant for which exposure, so it does not tell you which class suits a Pennsylvania winter. If you are specifying clay pavers for a place that freezes, ask the supplier which class and which standard the unit meets, and ask for the test data.

Color, sealing and efflorescence

The two sides make different claims here. BIA says clay color is fired through the body of the unit at almost 2000 degrees F and does not fade or require sealers. CMHA says concrete pigment is mixed in during production and that traffic, weather and dirt change the surface color over time, which cleaning and sealing can slow. CMHA adds that efflorescence can make concrete pavers look faded even though the color has not actually faded, and that dark pavers show it more than light ones. Efflorescence is not exclusive to concrete: the Construction Specifier article says soluble salts can come from brick, mortar or concrete, and that it needs salts, moisture, a path to the surface and evaporation. It also says powdery deposits can often be brushed off but can become crystalline and bond tightly with repeated wetting and drying. See our plain-language entry on efflorescence and our comparison of sealed vs unsealed pavers.

Where the sources disagree or go quiet

The strongest claims on the clay side come from the Brick Industry Association, a trade group for clay brick manufacturers, and the strongest claims on the concrete side come from CMHA, a trade group for concrete masonry. Neither compares the two products with independent test data. BIA calls clay much stronger and more durable than concrete, yet the two standards share an 8,000 psi average for SX clay and for concrete, and BIA’s own 10,000 psi figure is a description of most products, not a standard limit. No Penn State or other university source we found compares the two, and the one university page on brick paving, from the University of Missouri, covers hard-burned common brick set on a crushed stone and sand base, not manufactured clay pavers and not concrete. None of the sources gives installed cost, expected lifespan in years, or a Pennsylvania field result.

When each one fails

Concrete pavers fail when
  • Soil backfill or flat landscape edging is used as the edge restraint; CMHA says soil is never suitable and flat edging lacks lateral support (CMHA PAV-TEC-003).
  • Cleaning is careless; CMHA says it can damage or discolor the surface and that strong acids can slightly change paver color (PAV-TEC-005, 006).
  • Settlement occurs from poor compaction beside curbs or utility collars (PAV-TEC-003).
Clay pavers fail when
  • The class is not checked; C902 absorption limits run from 8 percent for SX to no limit for NX (BIA Technical Note 14 excerpt).
  • Moisture and salts have a path to the surface; the Construction Specifier names poor drainage and unprotected bases under pavers among efflorescence cases.
  • The sources give no other clay failure modes, so this list is short on purpose.
The sources do not settle
  • Which one lasts longer in Pennsylvania freeze-thaw and salt.
  • Which one costs less installed.
  • How clay pavers are repaired or edged.

Related

See our guides to clay brick pavers, brick vs concrete pavers in more detail, permeable vs standard pavers, pavers vs flagstone patio and edge restraint.

Questions

Are clay pavers stronger than concrete pavers?

The standards give both an 8,000 psi average at the top end: ASTM C936 for concrete and Class SX under ASTM C902 for clay. The Brick Industry Association says most clay pavers exceed 10,000 psi, which is an industry statement, not a standard limit.

Do clay pavers fade and do they need sealer?

The Brick Industry Association says clay color is fired through the unit and does not fade or require sealers. CMHA says concrete pavers change surface color gradually and that sealing can slow it. Neither gives long-term field data.

Do both kinds get efflorescence?

CMHA says it occurs on concrete pavers and is not structural. The Construction Specifier says soluble salts can come from brick, mortar or concrete, so brick can show it too.

Which costs less?

None of the sources compares price, so this page does not say. Verify against the current source and get written quotes for the same pattern and base.

Sources

Checked Nov 23, 2026. Verify against the current source. Planning information, not an engineering design. Muthler Landscaping & Construction LLC · 913 Bellefonte Ave, Lock Haven, PA 17745 · (570) 397-9800 · PA HIC #PA212584.