Sealing pavers is optional. The Concrete Masonry and Hardscapes Association (CMHA) lists sealers as an optional accessory, and its maintenance guide says what they can and cannot do. The main rule is order of work: clean first, deal with efflorescence, then seal.

Is sealing required?

No. CMHA’s guide specification for interlocking concrete pavement lists cleaners and sealers under optional accessories and treats cleaning or sealing as an optional step at the end of construction. Plenty of patios are never sealed. Whether it is worth doing depends on the site: how much dirt, oil or food the surface sees, how much the color matters to you, and how willing you are to maintain it.

What CMHA says sealers do

In its Operation and Maintenance Guide, CMHA says sealers:

  • Reduce water, stain, oil and dirt intrusion, and are useful near barbecues, trash receptacles, fast food restaurants and driveways.
  • Moderate color fading.
  • Help keep dirt from lodging in the surface, keep weed seeds from germinating, and keep ants out.
  • Can help hold sand in the joints; they are applied as a liquid over the paver surface and must soak in and cure.

Sealers may need to be reapplied “from time to time” because of wear and weather. CMHA gives no interval, so ask the sealer manufacturer for theirs.

Sealer chemistry and curing (CMHA PAV-TEC-005)

CMHA’s separate tech note on cleaners and sealers describes sealers by chemistry. Silanes and siloxanes penetrate and then cure in the concrete’s capillaries, forming a moisture barrier while letting the concrete breathe. Acrylics and urethanes stay largely on the surface and produce a gloss. Water-based epoxies penetrate deeply and leave a slight sheen. Solvent-based sealers carry dissolved solids as deep as the solvent penetrates, while water-based sealers are emulsions that penetrate only as far as their particle size allows.

The note says sealers do not add structural capacity. It calls for at least 24 hours without moisture or surface dampness before application, and for keeping traffic off until the sealer is dry, typically 24 hours. It warns against over-applying, because the surface can become slippery once cured. Sealing over a wet surface or a source of efflorescence can cause whitening. Acrylics generally last a few years before recoating, and urethanes cannot be rejuvenated by recoating.

The right order: clean, fix efflorescence, then seal

CMHA says to clean pavers first and seal after efflorescence is under control. Sealing follows stain removal, efflorescence removal and general cleaning. If efflorescence is a recurring concern, CMHA recommends a breathable sealer. For what efflorescence is, see efflorescence on pavers.

Limits to keep in mind

  • Reapplication is part of the deal: CMHA says sealers may need to be reapplied because of wear and weather.
  • CMHA’s maintenance guide does not address sealer types such as film-forming versus penetrating, or their effect on slip resistance. It says only that slip resistance depends on surface texture and joint width. Ask the manufacturer how a given sealer affects traction when wet.

Timing and weather

New pavers, joint sand and weather all affect when a sealer can go on, and the sealer’s label governs. We cover waiting times on how long to wait to seal pavers, and the joint sand and sealer calculator estimates gallons. De-icer choice matters on sealed and unsealed surfaces alike: CMHA says rock salt (sodium chloride) is the least damaging, calcium chloride can be used judiciously, and magnesium chloride and CMA are not recommended because they can chemically degrade all concrete types. See ice melt and paver warranties.

Questions to ask before you seal

  • Does the paver manufacturer’s warranty say anything about sealing, or about which sealers are allowed?
  • Is the sealer breathable, and what does the label say about efflorescence?
  • What is the finish: natural look or wet look, and how does it affect traction?
  • What is the reapplication schedule, and what does the product need to cure before foot traffic or rain?

Related

All hardscape materials · Polymeric sand explained · Concrete pavers explained · Pavers and patios guide

Get a quote

FAQ

Do pavers have to be sealed?

No. CMHA treats sealing as optional. It can reduce water, stain, oil and dirt intrusion and moderate color fading, but it is a maintenance decision.

Should I seal before or after cleaning?

After. CMHA says sealing follows stain removal, efflorescence removal and general cleaning.

What kind of sealer if efflorescence keeps coming back?

CMHA recommends a breathable sealer where efflorescence is a recurring concern.

How often do pavers need resealing?

CMHA says reapplication may be needed from time to time because of wear and weather, but gives no interval. Use the sealer manufacturer’s recommendation.

How dry should pavers be before sealing?

CMHA’s tech note on sealers says to allow at least 24 hours without moisture or surface dampness before application, and to keep traffic off until the sealer is dry, typically 24 hours.