Sealing concrete
For exterior concrete in a freeze-thaw climate, the sealer that the industry guidance points to is a breathable water repellent, not a shiny film. This page pulls together what the National Ready Mixed Concrete Association (NRMCA) and the Pennsylvania Aggregates and Concrete Association (PACA) say about sealers, when to apply one and what a sealer cannot do.
Which type of sealer
NRMCA’s guidance on scaling says to use a silane- or siloxane-based breathable sealer or water repellent designed for concrete slabs, and to follow the manufacturer’s directions. Breathable matters because moisture vapor needs to leave the slab. NRMCA does not name brands, and neither does this page; read the product’s data sheet for coverage, number of coats and reapplication, because the sources do not give a universal schedule.
What a sealer does and does not do
| A sealer can | A sealer is not |
|---|---|
| Help keep moisture in the slab so it keeps gaining strength as it cures (PACA). | A substitute for air-entrained, adequate-strength concrete. NRMCA lists non-air-entrained concrete and low strength as causes of scaling. |
| Help prevent chloride-laden moisture from migrating into the slab (PACA). | Permission to use de-icers freely. NRMCA and PACA both advise avoiding them on new concrete. |
| Add a layer of protection to the surface of a sound slab. | A repair for a slab that is already flaking. The surface must be sound for anything to bond. |
When to apply
NRMCA says the concrete should be reasonably dry before application, and calls late summer, after a few dry days, an ideal time. The NRMCA sheet gives no minimum concrete age or waiting period in days, so ask the sealer manufacturer, and keep in mind that curing compounds and sealers are different products. A freshly poured slab is still curing; the general timeline is in how long concrete takes to cure. Do not seal over a surface that is wet, dirty or still shedding powder.
Sealer, salt and the first winter
Both sources are direct about de-icers. NRMCA says to avoid them on new concrete if possible and use clean sand for traction, to use moderate amounts when needed, and to hose off salt that vehicles leave on driveways and garage slabs. It lists calcium chloride and sodium chloride (rock salt) as acceptable and says never to use ammonium sulfate, ammonium nitrate or magnesium-based salts. PACA goes further: de-icers should never be used on concrete that has not fully cured, and generally not in the pavement’s first year. Poor drainage that lets salt solutions pool makes scaling worse. For more on freeze-thaw flaking, see concrete spalling and scaling.
What to build in before you ever seal
- NRMCA recommends 4,000 psi concrete for exterior slabs that will stay moist, freeze and receive de-icers, and 3,500 psi if the slab will not stay continuously moist or receive de-icers.
- It recommends air-entrained concrete with 6 percent total air for 3/4-inch or 1-inch coarse aggregate. See 3000 vs 4000 psi concrete.
- Do not add water on site, avoid steel trowels, and cure with a pigmented liquid membrane compound or wet burlap and plastic sheeting.
Questions to ask
- Which sealer product, and is it breathable?
- When will it be applied, and what dryness does the manufacturer require?
- When will it need reapplying, per the data sheet?
Sources
- NRMCA, CIP 2, Scaling Concrete Surfaces (checked Nov 23, 2026)
- PACA, Scaling information sheet (checked Nov 23, 2026)
Related
Concrete spalling · How long before you can drive on new concrete · All concrete guides
FAQ
What type of sealer is recommended for exterior concrete?
NRMCA recommends a silane- or siloxane-based breathable sealer or water repellent designed for concrete slabs, applied per the manufacturer’s directions.
When should I seal new concrete?
NRMCA says the concrete should be reasonably dry and calls late summer after a few dry days ideal. It gives no minimum age, so follow the sealer manufacturer’s instructions.
Does sealing make it safe to use salt?
No source says so. NRMCA advises avoiding de-icers on new concrete, and PACA recommends none in the first year and never on uncured concrete.
What de-icers should never touch concrete?
NRMCA says never use ammonium sulfate, ammonium nitrate or magnesium-based salts; PACA also says never to use ammonium sulfate or ammonium nitrate.
Planning information only, not engineering advice. Follow the sealer manufacturer’s data sheet and your contractor’s instructions. Sources checked Nov 23, 2026.